Products

  • Medium temperature asphalt block

    Medium temperature asphalt block

    Indicator requirements:

    Softening point: 50-70 ℃

    ash content: ≤ 0.5%.

    Product features and uses: This type of asphalt has a low softening point and is generally used for blending oil in coking goods. Low temperature asphalt belongs to special asphalt and can also be used for asphalt paint, recycled rubber, rubber products, waterproof materials, anti-corrosion, paving, etc. Our factory can produce according to customer demand indicators.

    Soft Pitch is the residue of tar distillation, with a yield of 54-56% of tar. It is composed of aromatic compounds with more than three rings, oxygen-containing, nitrogen-containing, sulfur-containing heterocyclic compounds, and a small amount of high molecular weight carbon substances. The molecular weight of asphalt components ranges from 200 to 2000, with a maximum of 3000. Medium temperature asphalt is classified based on different softening points. The softening point is 60-80 ℃ for medium temperature asphalt.

  • Special asphalt for oilfield additives

    Special asphalt for oilfield additives

    Oil solubility: ≥ 95%

    Appearance: Black powder.

    Product specifications: 25 kg/bag.

    Packaging and storage: Store in a cool, dry, and ventilated place, moisture-proof, and sunproof.

    Safety precautions: Avoid contact with eyes, skin, and clothing, otherwise rinse with plenty of water.

    Our factory produces 300 tons of asphalt per day and can customize the production of asphalt according to customer needs.

    Product use: Asphalt powder can play an anti collapse role in drilling fluids, fill pore throats and cracks, and seal them. It can also cover shale interfaces, improve mud cake quality, lubricate, and reduce high-temperature and high-pressure filtration loss

  • Petroleum asphalt flakes

    Petroleum asphalt flakes

    Product indicator requirements:

    Softening point: 90-110 ℃

    Ash content: ≤ 0.1%

    Residual carbon: ≥ 55%

  • Ball pitch

    Ball pitch

    Indicator requirements:

    Softening point 120 ℃

    Ash content ≤ 0.3%

    Volatile content ≤ 56%

    Carbon content ≤ 50%

    Coking value ≤ 60%

    Particle size 0.2-1 mm

  • Coal tar pitch flakes

    Coal tar pitch flakes

    Product indicators:

    Softening point: 140-155 ℃

    Ash content: around 14%

    Fixed carbon: 45%

    Sulfur content: around 1.35%

    Low heat level: 7300

    High heat level: 8200

  • Asphalt powder

    Asphalt powder

    Indicator requirements:

    Softening point: 105-155 ℃

    Ash content: ≤ 0.5%

    Coking value: ≥ 55%

  • National standard medium temperature asphalt

    National standard medium temperature asphalt

    Indicator requirements:

    Softening point: 80-90 ℃

    Ash content: ≤ 0.3%

    Coking value: ≥ 50%

    Volatility: 58-62%

    Insoluble substances in toluene: 15-25%

    Quinoline insoluble substances: 4-10%.

  • High temperature coal tar

    High temperature coal tar

    Density 1.18-1.22

    Ash content ≤ 0.3%

    Water ≤ 4%

    Viscosity E80 ≤ 4.2%

    Sulfur content ≤ 1%

    Toluene insoluble substance ≤ 9%

    Asphalt content 50-60%

  • High temperature asphalt

    High temperature asphalt

    Indicator requirements:

    Softening point: 120-150 ℃

    Ash content: ≤ 1%

    Coking value: ≥ 55%

    Volatility: 50-65%

    Moisture content: ≤ 5%

  • Modified asphalt

    Modified asphalt

    Product indicators

    Softening point: 105-115 ℃

    Ash content: ≤ 0.3%

    Volatility: 48-54

    Coking value: ≥ 57%

    Fixed carbon: ≥ 50%

    Moisture: < 5%

    Sulfur content: ≤ 0.5%

    Toluene insoluble substance: 28-32%

    Quinoline insoluble substances: 6-12%